I'll bet those zincs work fine, as they sit. no need to mess with zinc for a number of years.
We had the same problem with the heat exchanger zincs breaking/wearing off. When we changed to aluminum anodes, we also changed the one on our heat exchanger to one manufactured by Peformance Metals. They have a wire core and so far I haven’t have any break off when they get changed.
Hey... that is pretty slick!
Question about loctite or even anti-seize. Do you or do you not need to have a very good connection to ground for them to work? Would not substances hinder such a connection?
(Asking for a friend.) ;-)